Protective Clothing

CHEMICAL PERMEATION / PENETRATION TESTING
ASTM F1001 Recommended List of Chemicals Fpr Evaluating Protective Clothing Materials (ASTM F739)

Chemical Penetration Testing (ASTM P903)
Challenge
Chemical
Average Normalized
Breakthrough Time
(minutes)
Average
Permeation Rate
(ug/cm2/minute)
Penetration
Results
Acetone80.62PASS
Acetonitrile<48.7PASS
Ammonia44.5N/T
1,3-Butadiene811.9N/T
Carbon Disulfide<4<50PASS
Chlorine Gas62.3N/T
Dichloromethane40.59PASS
Diethylamine49.5PASS
N,N-Dimethylformamide82.1PASS
Ethyl Acetate42.3PASS
Ethylene Oxide<4359N/T
n-Hexane46.3PASS
Hydrogen Chloride30>50N/T
Methanol<42.23PASS
Methyl Chloride40.38N/T
Nitrobenzene416PASS
Sodium HydroxideNDNDPASS
Sulfuric AcidNDNDPASS
Tetrachloroethylene810PASS
Tetrahydrofuran<4<50PASS
Toluene4825PASS
Breakthrough Time is taken between the first contact of the chemical with outer layer of the fabric and its direction on the inside. Permeation rate is the constant rate of permeation that occurs after chemical breakthrough occurs and all factors affecting the permeation have reached their equilibrium state.


COMPARATIVE COMPOSITE DATA SHEET
PropertyMethodPOSI-WEARTMTyvek® Grade 1422A
Weight (oz/yd2)ASTM D-19101.711.15
Thickness (mils)ASTM 1777*64105
Tensile Strength (lbs.) MDASTM D-16823417
Tensile Strength (lbs.) CDGrab1918
Tensile Strength (lbs.in) MDASTM D-1682107
Tensile Strength (lbs.in) CDStrip69
Trapezoid TearASTM D-2263>105
Trapezoid Tear (lbs.) CD>76
Bond Strength (lbs.) MDIST 110*2*82Min. 1.0Not Applicable
Bond Strength (lbs.) CDMin. 1.0Not Applicable
Hydrostatic Head (cms)>100<75
Moisture Vapor Trans.ASTM F-1249Not ApplicableLOW
Resistance to Penetration
by Liquids (2 psi)
ASTM ES-21PASSNot Applicable
Posi-WearTM test data taken from POLY-BOND, INC. labs and independent test labs.
Posi-WearTM is manufactured from the material POLY-SAFE, which is manufactured by POLY-BOND, INC.



Close Window

 Click here for home   Click here for order page